TESTING RESULT
The Simulation of Real World - Cyclical Seawater Immersion for 40 Days Corrosion Results (Cyclic Corrosion Testing)
The Test Results for 40 Days Seawater Immersion Corrosivity (Phase 1)The Self-Drilling Screws Test Results for 40 Days Seawater Immersion Corrosivity | |
Test Start Date | At 3:00 on September 24th, 2015 |
Sample QTY | 5 Pieces/Per Different Self-Drilling Screw |
Test Cycle Time Per Stage | (Initial Period): 7 days’ immersion in seawater, and then another 3 days’ exposure to the sun (till 4th October, 2015). (Midterm): 2 days’ exposure to the sun after 3 days’ soaking in seawater, and this cycle was to repeat 4 times. (Final): 3 days’ exposure to the sun after 7 days’ soaking in seawater. The test ends at this stage. |
Total Test Cycle Time | 40 Days |
Picture 1: The Test Result Overview Picture for 4 Kinds of Self-Drilling Screws
Picture 2: XIOD Coating Highly Corrosion Resistant Self-Drilling Screws(It Has Been Drilled)
Picture 3: XIOD Coating Highly Corrosion Resistant Self-Drilling Screws(Whole Brand New)
Picture 4: #410 Stainless Steel Self-Drilling Screws(Whole Brand New)
Picture 5: #302 SS Head Self-Drilling Screws(Whole Brand New)